How you ever seen 3” PVC Pipe Heated up and Bent Manually? Father and Son Electricians do, Thoughts?
What happens here
An issue arose where the back-to-back 90-degree bend was not perfectly straight; the pipe was observed to be crooked between the bends. To rectify this, the misaligned section of the PVC pipe is re-inserted into the 1000-degree hot box to re-heat and soften it. Once pliable, the pipe is carefully straightened by hand while still hot, with the assistance of a helper to ensure it cools and hardens in a perfectly straight line.
Goal: Correct a crooked back-to-back 90-degree bend.
Tools and materials
- Heat-resistant Gloves — Protecting hands from high heat
- Helper — Assisting with holding the pipe straight during cooling
- Misaligned 3-inch PVC Pipe — The pipe requiring correction